Engineering Materials·MCQ explained

An aggregate particle is said to be flaky if its minimum dimension is less than

Try it first: pick an option, then read the explanation.

Correct answer: C. 3/5th of mean length

Detailed Explanation: Flakiness Definition (IS 2386 Part I)

The flakiness criterion is one of the most frequently tested aggregate definitions in civil engineering examinations. The threshold of 3/5th (0.6 times) the mean sieve size is fixed by IS 2386 (Part I) and does not change regardless of the size fraction being tested.

Why C (3/5th = 0.6) is correct: By IS 2386 Part I, a particle is “flaky” if its least dimension (thickness) is less than 0.6 × the mean of the upper and lower sieve sizes defining its fraction. This 3/5 = 0.6 factor is a fixed standard value. Option A (1/5 = 0.2) is too small; Option B (2/5 = 0.4) is incorrect; Option D (4/5 = 0.8) would include too many particles. The standard uses exactly 3/5.

Flakiness vs. Elongation Criteria

Shape TestCriterionFactor
Flakiness IndexMin dimension < 0.6 × mean sieve size3/5 = 0.6
Elongation IndexMax dimension > 1.8 × mean sieve size9/5 = 1.8

Key Concepts for Students

  • Flakiness factor = 3/5 = 0.6; Elongation factor = 9/5 = 1.8 — these two numbers define the shape tests.
  • Flakiness index should be ≤35% by mass for aggregate used in concrete (IS 383).
  • High flakiness index causes segregation, poor workability, and lower concrete strength due to weak aggregate orientation under load.