Engineering Materials·MCQ explained

As per IS 7861 (Part 2), concreting done at atmospheric temperature ________ or below is termed as cold weather concreting.

Try it first: pick an option, then read the explanation.

Correct answer: B. 5°C

Detailed Explanation: IS 7861 Part 2 — Cold Weather Concreting Threshold

Why B (5°C) is correct: IS 7861 (Part 2) sets the cold weather concreting threshold at 5°C atmospheric temperature or below. Below this temperature, hydration rate drops dramatically and water in the mix risks freezing before the concrete gains adequate strength. If water freezes before sufficient hydration, the expansion (~9% volume increase on freezing) damages the concrete matrix permanently.

Why 5°C Is Critical

TemperatureEffect on Hydration
20°C (reference)Normal hydration; standard strength development
10°CHydration rate slowed by ~50%; curing period extended
5°CHydration nearly stops; cold weather precautions mandatory (IS 7861 Part 2)
0°C (freezing)Free water freezes; expansion causes micro-cracking; irreversible damage
<0°CSevere damage; concrete may be permanently weakened

IS 7861 Part 2: Precautions for Cold Weather Concreting

PrecautionDetail
Minimum placement temperatureNot less than 4.5°C
Minimum temperature during hardeningMaintain above 2°C until concrete achieves design strength
Accelerating admixtureCalcium chloride (CaCl2) up to 2% by weight of cement (OPC only)
Cement type preferredHigh C3S content (e.g., OPC 53 grade) for faster early strength
Avoid salts/anti-freeze chemicalsGenerally not recommended as they degrade concrete quality
Heated water / aggregatesWarm the mix to ensure adequate reaction temperature
  • Cold weather threshold per IS 7861 (Part 2) = 5°C or below.
  • Cement preference: high C3S, low C2S for faster early strength in cold.
  • Freezing water expands ~9% by volume — this is why preventing freezing before adequate strength is paramount.