Too wet a concrete may cause:

Using a too-wet (high w/c) concrete mix may cause:

A. Segregation
B. Concrete of lower density
C. Concrete of lower strength
D. All of these
Correct Answer: D. All of these

📚 Detailed Explanation: Effects of Excessively Wet Concrete Mix

Why D (All of these) is correct: Excess water in a concrete mix creates a cascading series of problems. Lower paste viscosity reduces cohesion (segregation risk), excess evaporation leaves large capillary voids (lower density and strength), and a higher w/c ratio directly reduces compressive strength per Abrams' Law.

Three Consequences of a Too-Wet Mix

Consequence Mechanism Quantified Impact
A. Segregation Excess water lowers paste viscosity and yield strength; cannot suspend dense aggregate particles which sink under gravity 5% voids from segregation → >30% strength loss
B. Lower density Excess water occupies space in the mix; evaporates after hardening leaving capillary pores and voids; concrete becomes more porous and lighter Density can drop from ~2400 kg/m³ to 2250 or less
C. Lower strength Abrams' Law: compressive strength is inversely proportional to w/c ratio; more water directly dilutes the paste quality; more voids form on evaporation Doubling w/c from 0.4 to 0.8 can reduce strength by 50%+
Abrams' Law (approximate):
f = K1 / K2^(w/c)
where:
f = compressive strength
K1, K2 = empirical constants (≈ 97 MPa and 4.0 for typical conditions)
w/c = water-cement ratio

Result: Every 0.1 increase in w/c reduces strength by ≈ 15–20%

Water-Cement Ratio vs. 28-day Strength (M25 concrete)

w/c Ratio 28-day Strength (MPa) Remarks
0.40 38–42 Rich, low-water mix; excellent durability
0.50 30–35 Standard M25 design w/c
0.60 22–28 Adequate for M20 if other factors controlled
0.70 16–20 Lean, wet mix; not recommended for structural concrete
0.80 10–14 Very wet; high segregation; not suitable
  • Too-wet concrete causes: segregation, lower density, and lower compressive strength (all simultaneously).
  • IS 456:2000 maximum w/c ratios: 0.45 for moderate exposure; 0.40 for severe exposure.
  • Never add water at the site to “improve workability” — this is a code violation and causes all three defects.

← Back to MCQs on Physical Quality of Concrete

Leave a Comment

Your email address will not be published. Required fields are marked *

Scroll to Top