Home/MCQ Practice/Concrete Technology MCQs/Workability of Concrete

Engineering Materials·MCQ practice

MCQs on Workability of Concrete – Page 3

15 questions. Tap an option to check it instantly, then read the solution.

MCQs on Workability of Concrete — Page 3

Question 1Easy
In a slump test, each layer of concrete is compacted by a steel rod 60 cm long and of 16 mm diameter for:
Full explanation

Answer: B. 25 times

As per IS 1199, each of the three layers of concrete in the slump cone is rodded (tamped) 25 times with the standard tamping rod (16 mm diameter, 600 mm long, bullet-nosed end). This ensures uniform compaction of each layer.
Question 2Easy
What is the range of slump (mm) of the concrete which is used as the mass concrete?
Full explanation

Answer: B. 20 to 50

Mass concrete (large unreinforced or lightly reinforced pours such as dam bodies, foundations, retaining walls) uses a low slump of 20-50 mm. Low workability is possible because the large cross-section is easy to vibrate and lower w/c reduces heat of hydration.
Question 3Easy
The main object of compaction of concrete is:
Full explanation

Answer: D. All options are correct

All three objectives are equally valid. Compaction serves to: (a) eliminate entrapped air voids; (b) achieve maximum density by expelling air and water pockets; (c) ensure the concrete fills all spaces around reinforcement bars, formwork corners, and embedded items.
Question 4Medium
Which of the following statements is false?
Full explanation

Answer: A. Workability of the concrete mix decreases with an increase in the moisture content

Statement (a) is FALSE. Workability INCREASES with an increase in moisture (water) content, not decreases. More water in the mix increases fluidity and lubrication, reducing inter-particle friction. Statements (b) and (c) are correct.
Question 5Easy
How many hoppers are in compaction factor test of concrete?
Full explanation

Answer: C. 2

The Compacting Factor Apparatus (IS 5515) has 2 hoppers (one upper and one lower) stacked above a cylinder. The concrete falls from the upper hopper through the lower hopper into the cylinder, achieving partial compaction by gravity.
Question 6Easy
The slump test is performed to check the -
Full explanation

Answer: D. Workability of concrete

The slump test (IS 1199) is a field test performed on fresh concrete specifically to assess its workability (consistency). It measures the degree of fluidity of the mix.
Question 7Easy
Pick up the correct statement from the following.
Full explanation

Answer: D. All options are correct

All three statements are correct. Unexpectedly high workability on site may indicate excess water or moisture (A). It may also indicate insufficient sand (B) as a rich cement-paste mix will flow more easily. A completely dry (earth-moist) mix will show zero slump (C).
Question 8Easy
The entrained air in concrete ..................
Full explanation

Answer: A. Increases workability

Entrained air (intentionally introduced tiny air bubbles via air-entraining agents) increases workability because the microscopic spherical air bubbles act as a ball-bearing lubricant between aggregate particles, reducing internal friction.
Question 9Medium
The workability of concrete can be improved by:
Full explanation

Answer: B. More cement

Increasing cement content (while maintaining the same w/c ratio) increases the total paste volume, which provides better lubrication of aggregate particles and improves workability. More fine aggregate or sand increases surface area and reduces workability. Finer coarse aggregate also increases surface area.
Question 10Easy
The top diameter, bottom diameter and the height of a slump mould are ..........
Full explanation

Answer: A. 10 cm, 20 cm, 30 cm

The slump cone dimensions per IS 1199 are: Top diameter = 10 cm (100 mm), Bottom diameter = 20 cm (200 mm), Height = 30 cm (300 mm). The top is the smaller opening and the bottom is the larger base.
Question 11Hard
Pick up the incorrect statement from the following.
Full explanation

Answer: A. A rich mix of concrete possesses higher strength than that a lean mix of desired workability with excessive quantity of water

Statement (a) is incorrect because strength depends solely on the water-cement ratio (Abrams' Law), not on whether the mix is rich or lean. A lean mix with a properly controlled (low) w/c ratio can have equal or higher strength than a rich mix. Richness alone does not guarantee superior strength.
Question 12Medium
Pick up the correct statement from the following.
Full explanation

Answer: D. None of these

All three statements (a), (b), (c) are false. Segregation is HARMFUL (not necessary) for workable concrete. Consistency directly affects workability. Higher slump means higher workability (not lower). Therefore the correct choice is 'None of these'.
Question 13Medium
For given water content, workability decreases if the concrete aggregates contain an excess of
Full explanation

Answer: D. All options are correct

Thin, flat, and elongated particles all decrease workability because they have a high surface-area-to-volume ratio (more water needed to coat them) and they interlock and bridge, creating more mechanical resistance to flow.
Question 14Medium
The test most suitable for concrete of very low workability is .................
Full explanation

Answer: C. Vee-Bee test

The Vee-Bee consistometer test is most suitable for very low workability concrete (VB time > 10 seconds). At very low workability, the slump is zero (slump test fails) and the compaction factor difference is too small for reliable discrimination.
Question 15Easy
A concrete having a slump of 6.5 cm is said to be ...........
Full explanation

Answer: D. plastic

A slump of 6.5 cm = 65 mm falls in the 50-100 mm range, which corresponds to medium workability — described as 'plastic' consistency in IS terminology. Plastic concrete flows and compacts readily.